Filament drying: how to spot wet plastic and save it

In 3D printing, moisture problems appear sooner or later. Plastics used for 3D printing are naturally hygroscopic. This means they absorb moisture from the air. Sometimes it takes weeks, but for some materials, a few hours on the desk is enough. We explain how to deal with this issue and prevent ruined prints.

Why filament absorbs moisture

A basic characteristic of most thermoplastics is their ability to bind water molecules from the surrounding air. It is not a manufacturing defect, but a physical property. Different plastics have different levels of hygroscopy. While standard PLA will stay in good condition on the desk for quite a long time, technical materials absorb water very quickly. Once water gets into the structure of the filament, it waits for the moment it passes through the hot nozzle. There it heats up rapidly, turns into steam and causes problems.

How to spot wet filament

The symptoms of damp filament are quite clear. The first and most common sign is popping and hissing during printing. A crackling sound can be heard. The water trapped in the plastic turns into steam in the nozzle, escapes and creates microscopic explosions. The result is bubbles on the surface of the print. The surface is then rough, matte and full of tiny craters.

Another typical manifestation is excessive stringing. Pulling thin threads during nozzle travel mainly affects PETG and TPU. Wet material flows from the nozzle differently and is harder to control with retractions. With PLA, moisture manifests itself in one more specific way. The filament becomes extremely brittle. If PLA snaps while being loaded into the extruder or breaks on its own on the spool, it is full of moisture.

Table of drying temperatures and times

Each material requires a different drying temperature. If the setting is too low, the water will not evaporate. If the setting is too high, the spool will melt together. Here are the values we recommend and test on our own printers.

Material Drying temperature Drying time
PLA 45 °C 4 to 6 hours (if brittle)
PLA+ 45 °C Typically 4 to 6 hours
PETG 65 °C 4 to 6 hours
PCTG 65 °C 4 to 6 hours
ABS and ASA 80 °C Approximately 4 hours
TPU 50 to 55 °C 4 to 8 hours
Nylon PA12 70 °C 8 hours (before every print)

Drying temperature by material

The temperature and time we recommend and use on our printers.

PLA
45 °C · 4 to 6 h
PLA+
45 °C · 4 to 6 h
TPU
50 to 55 °C · 4 to 8 h
PETG
65 °C · 4 to 6 h
PCTG
65 °C · 4 to 6 h
PA12
70 °C · 8 h
ABS, ASA
80 °C · about 4 h
0 °C30 °C60 °C90 °C

Never dry above the temperature at which the material softens. The spool could deform.

How to dry correctly

The best choice is a specialized filament dryer. It maintains a stable temperature, has a timer and often a fan that vents the moist air out. Another good and cheaper alternative is a food dehydrator. It is enough to cut out the centers of the trays so that the whole spool fits inside. It works absolutely reliably.

Questions often arise about drying in a baking oven. An oven poses a huge risk and we do not recommend it. Most domestic ovens have massive temperature fluctuations. A setting of 50 degrees can easily result in the heating element warming the interior to 80 degrees for a moment before the thermostat reacts. The result is a deformed spool and melted plastic that must be thrown away.

eSUN eBOX Lite filament drying box
eSUN eBOX Lite drying box. Filament can be dried in it and printed directly from it.

Storage after drying

Once the spool is dried, it must be stored correctly. Leaving it on the desk will cause it to absorb moisture again soon. We recommend sealable plastic boxes with a rubber seal. Simply pour silica gel into the bottom, which absorbs residual moisture from the air inside the box. It is a cheap and very effective solution.

For very sensitive materials, such as Nylon PA12, standard storage is not enough. This material absorbs moisture so quickly that it would spoil even during a longer print. Therefore, it is necessary to print it directly from a dryer or a dry box, which protects the filament all the way to the extruder.

Frequently asked questions (FAQ)

1. Is a new, vacuum-sealed spool always dry?

No. Manufacturers often cool the filament during production in a water bath. If it is insufficiently dried before being packed into a vacuum bag, wet filament will be delivered. This happens even with premium brands.

2. Can wet PLA be printed?

Sometimes yes, but the surface quality will be worse and the part will be more brittle. If the filament pops and forms bubbles, it is better to dry it. This prevents a ruined print.

3. How long does silica gel last in a box?

It depends on how often the box is opened and what the humidity in the room is. Typically, it lasts several months. We recommend using silica gel with a moisture indicator. Once it changes color, it can be dried and used again.

4. Can filament be dried on the heated print bed?

It is possible. The spool is placed on the bed, the correct temperature is set and it is covered with a cardboard box with a few holes made for moisture venting. However, it is more of an emergency solution if a dryer is not available.

5. Does popping in the nozzle always mean moisture?

Mostly yes. Sometimes, however, it can be a poorly set retraction where air gets into the nozzle, or a printing temperature that is too high, causing the material to boil. But if bubbles on the surface and excessive stringing are also visible, it is clearly moisture.